MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 2170HG High Impact ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: ALLEN® 2160HG is a general purpose ABS that has high impact strength and a good cost to performance ratio to other materials like painted metal, FRP, aluminum, and other thermoplastics.

ALLEN® 2160HG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Marie products
  • Recreational vehicles
  • Agricultural cab interiors
  • Truck interiors
  • Equipment covers
  • POP Displays
Features:
  • Custom color matching
  • Ease of processing
  • Regrind compatible in future orders
  • High gloss finish
  • UV protective films available

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Water Absorption 0.310 %0.310 %24; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 99.099.0ASTM D785
Tensile Strength 34.9 MPa5060 psiASTM D638
Tensile Modulus 2.034 GPa295.0 ksiASTM D638
Flexural Strength 53.4 MPa
@Strain 5.00 %
7750 psi
@Strain 5.00 %
ASTM D790
Flexural Modulus 1.82 GPa264 ksiASTM D790
Compressive Yield Strength 47.5 MPa6890 psiASTM D695
Bearing Yield Strength <= 171.7 MPa<= 24900 psiASTM D953
 20.3 MPa
@Strain 4.00 %
2940 psi
@Strain 4.00 %
ASTM D953
Shear Strength 37.4 MPa5420 psiASTM D732
Izod Impact, Notched 2.776 J/cm5.201 ft-lb/inASTM D256
Gardner Impact 16.7 J12.3 ft-lbDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.3 kV/mm414 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 84.0 µm/m-°C46.7 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °Fannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0598 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS555 / 325295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.