MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Esprix Ketoprix™ EKT33G2L Thermoplastic Aliphatic Polyketone, Fiber Reinforced Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyketone, Glass Fiber Reinforced

Material Notes: Ketoprix™ EKT33G2L and EKT33G3L resins are thermoplastic aliphatic polyketone compounds where the polyketone base polymer consists of perfectly alternating a-olefins and CO to give the 1,4-diketone polymer backbone structure. To this base resin, fiber reinforcement, additional thermal stabilizers and lubricants are added to achieve desired mechanical performance and to assist in injection molding. These compounded resins are formulated for Injection Molded parts where higher strength and stiffness are required. Ketoprix™ EKT23G3C2/3 compounds are typically used in E&E, Automotive and Industrial End Uses.

Information provided by Esprix Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D 792
Viscosity 100000 - 300000 cP
@Temperature 280 °C
100000 - 300000 cP
@Temperature 536 °F
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 - 90.0 MPa
@Temperature 23.0 °C
11600 - 13100 psi
@Temperature 73.4 °F
ASTM D 638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %Nominal; ASTM D 638
Tensile Modulus 6.00 - 7.00 GPa
@Temperature 23.0 °C
870 - 1020 ksi
@Temperature 73.4 °F
ASTM D 638
Flexural Strength 120 - 130 MPa
@Temperature 23.0 °C
17400 - 18900 psi
@Temperature 73.4 °F
ASTM D 790
Flexural Modulus 5.00 - 6.00 GPa
@Temperature 23.0 °C
725 - 870 ksi
@Temperature 73.4 °F
ASTM D 790
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D 1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PESPR910 / 217564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.