MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, PTFE Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, PTFE Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.08 - 1.60 g/cc0.0390 - 0.0578 lb/in³Average value: 1.30 g/cc Grade Count:122
Water Absorption 0.300 - 8.50 %0.300 - 8.50 %Average value: 0.944 % Grade Count:70
Moisture Absorption at Equilibrium 1.00 - 2.80 %1.00 - 2.80 %Average value: 1.29 % Grade Count:8
Water Absorption at Saturation 5.00 - 6.00 %5.00 - 6.00 %Average value: 5.21 % Grade Count:7
Additive Loading 5.00 - 15.0 %5.00 - 15.0 %Average value: 10.0 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.0450 cm/cm0.00100 - 0.0450 in/inAverage value: 0.0147 cm/cm Grade Count:109
Linear Mold Shrinkage, Transverse 0.00350 - 0.0260 cm/cm0.00350 - 0.0260 in/inAverage value: 0.0121 cm/cm Grade Count:16
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 90.0 - 12290.0 - 122Average value: 107 Grade Count:37
Ball Indentation Hardness 60.0 - 140 MPa8700 - 20300 psiAverage value: 115 MPa Grade Count:4
Tensile Strength, Ultimate 36.5 - 220 MPa5300 - 31900 psiAverage value: 74.7 MPa Grade Count:89
Tensile Strength, Yield 35.0 - 181 MPa5080 - 26200 psiAverage value: 109 MPa Grade Count:39
 131 - 131 MPa
@Temperature 93.3 - 93.3 °C
19000 - 19000 psi
@Temperature 200 - 200 °F
Average value: 131 MPa Grade Count:1
Elongation at Break 2.00 - 240 %2.00 - 240 %Average value: 9.76 % Grade Count:115
Elongation at Yield 2.00 - 40.0 %2.00 - 40.0 %Average value: 11.4 % Grade Count:14
Modulus of Elasticity 1.20 - 24.0 GPa174 - 3480 ksiAverage value: 3.57 GPa Grade Count:69
Flexural Yield Strength 45.0 - 303 MPa6530 - 44000 psiAverage value: 127 MPa Grade Count:114
Flexural Modulus 1.20 - 15.5 GPa174 - 2250 ksiAverage value: 4.21 GPa Grade Count:114
 8.96318 - 8.96318 GPa
@Temperature 93.3 - 93.3 °C
1300.02 - 1300.02 ksi
@Temperature 200 - 200 °F
Average value: 8.96 GPa Grade Count:1
Flexural Strain at Break 2.50 - 8.60 %2.50 - 8.60 %Average value: 6.00 % Grade Count:8
Compressive Yield Strength 30.3 - 68.9 MPa4400 - 10000 psiAverage value: 50.3 MPa Grade Count:8
Izod Impact, Notched 0.214 - 2.14 J/cm0.401 - 4.00 ft-lb/inAverage value: 0.707 J/cm Grade Count:90
Izod Impact, Unnotched 1.71 J/cm - NB3.20 ft-lb/in - NBAverage value: 8.60 J/cm Grade Count:49
Izod Impact, Notched (ISO) 2.60 - 16.0 kJ/m²1.24 - 7.61 ft-lb/in²Average value: 6.68 kJ/m² Grade Count:13
 8.00 - 11.0 kJ/m²
@Temperature -30.0 - -30.0 °C
3.81 - 5.23 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 9.50 kJ/m² Grade Count:2
Izod Impact, Unnotched (ISO) 10.7 - 80.0 kJ/m²5.09 - 38.1 ft-lb/in²Average value: 44.3 kJ/m² Grade Count:9
 45.0 - 70.0 kJ/m²
@Temperature -30.0 - -30.0 °C
21.4 - 33.3 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 57.5 kJ/m² Grade Count:2
Charpy Impact Unnotched 3.99 J/cm² - NB19.0 ft-lb/in² - NBAverage value: 6.46 J/cm² Grade Count:24
 2.94 J/cm² - NB
@Temperature -40.0 - -30.0 °C
14.0 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 5.00 J/cm² Grade Count:19
Charpy Impact, Notched 0.280 - 1.60 J/cm²1.33 - 7.61 ft-lb/in²Average value: 0.737 J/cm² Grade Count:27
 0.294 - 0.900 J/cm²
@Temperature -40.0 - -30.0 °C
1.40 - 4.28 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 0.553 J/cm² Grade Count:10
Falling Dart Impact 0.570 - 4.10 J0.420 - 3.02 ft-lbAverage value: 2.55 J Grade Count:5
Instrumented Impact Total Energy 0.740 - 4.20 J0.546 - 3.10 ft-lbAverage value: 1.58 J Grade Count:5
Coefficient of Friction 0.160 - 0.4100.160 - 0.410Average value: 0.249 Grade Count:19
Coefficient of Friction, Static 0.110 - 0.3400.110 - 0.340Average value: 0.200 Grade Count:19
K (wear) Factor 6.20 - 306 x 10-8 mm³/N-M3.08 - 152 x 10-10 in³-min/ft-lb-hrAverage value: 55.4 x 10-8 mm³/N-M Grade Count:20
Limiting Pressure Velocity 0.333 - 0.701 MPa-m/sec9500 - 20000 psi-ft/minAverage value: 0.587 MPa-m/sec Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+16 ohm-cm100 - 1.00e+16 ohm-cmAverage value: 1.32e+15 ohm-cm Grade Count:69
Surface Resistance 500 - 1.00e+14 ohm500 - 1.00e+14 ohmAverage value: 1.68e+13 ohm Grade Count:13
Dielectric Constant 3.60 - 3.703.60 - 3.70Average value: 3.63 Grade Count:4
Dielectric Strength 17.3 - 27.2 kV/mm440 - 690 kV/inAverage value: 20.3 kV/mm Grade Count:33
Dissipation Factor 0.0100 - 0.02000.0100 - 0.0200Average value: 0.0164 Grade Count:7
Comparative Tracking Index 450 - 600 V450 - 600 VAverage value: 535 V Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 - 120 µm/m-°C10.0 - 66.7 µin/in-°FAverage value: 52.8 µm/m-°C Grade Count:50
CTE, linear, Transverse to Flow 70.0 - 101 µm/m-°C38.9 - 56.0 µin/in-°FAverage value: 86.4 µm/m-°C Grade Count:4
Thermal Conductivity 0.230 - 0.418 W/m-K1.60 - 2.90 BTU-in/hr-ft²-°FAverage value: 0.259 W/m-K Grade Count:9
Melting Point 250 - 275 °C482 - 527 °FAverage value: 259 °C Grade Count:23
Maximum Service Temperature, Air 80.0 - 180 °C176 - 356 °FAverage value: 131 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 155 - 260 °C311 - 500 °FAverage value: 227 °C Grade Count:45
Deflection Temperature at 1.8 MPa (264 psi) 55.0 - 260 °C131 - 500 °FAverage value: 136 °C Grade Count:111
Deflection Temperature at 8.0 MPa 65.0 - 220 °C149 - 428 °FAverage value: 117 °C Grade Count:3
Vicat Softening Point 230 - 255 °C446 - 491 °FAverage value: 241 °C Grade Count:21
Flammability, UL94 HB - V-0HB - V-0Grade Count:69
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 300 °C500 - 572 °FAverage value: 284 °C Grade Count:15
Nozzle Temperature 280 - 300 °C536 - 572 °FAverage value: 290 °C Grade Count:8
Melt Temperature 260 - 310 °C500 - 590 °FAverage value: 290 °C Grade Count:58
Mold Temperature 40.0 - 121 °C104 - 250 °FAverage value: 89.2 °C Grade Count:70
Drying Temperature 75.0 - 105 °C167 - 221 °FAverage value: 83.6 °C Grade Count:57
Moisture Content 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.185 % Grade Count:40
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:24
Injection Pressure 4.96 - 128 MPa720 - 18600 psiAverage value: 92.4 MPa Grade Count:39

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Impact Grade
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66/6
Overview of materials for Nylon 6, PTFE Filled
Overview of materials for Nylon 66, MoS2 Filled

O2508 / 78007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.