MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Techtron™ HPV PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Unreinforced, Extruded

Material Notes: This internally lubricated, glass-fiber reinforced PPS bridges the gap in performance and price between standard and advanced engineering plastics, exhibiting excellent resistance to wear, hydrolysis, and chemicals, as well as great electrical insulation and low flammability.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Water Absorption at Saturation 0.0900 %0.0900 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 82.082.0ASTM D785
Hardness, Shore D 82.082.0ISO 868
Tensile Strength 78.0 MPa11300 psiISO 527-1/-2 (7)
Flexural Strength 118 MPa17100 psiISO 178 (12)
Compressive Yield Strength  33.0 MPa
@Strain 1.00 %
4790 psi
@Strain 1.00 %
ISO 604 (10)
 65.0 MPa
@Strain 2.00 %
9430 psi
@Strain 2.00 %
ISO 604 (10)
 105 MPa
@Strain 5.00 %
15200 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
 24.0 kV/mm610 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 µm/m-°C33.0 µin/in-°FASTM E-831 (TMA)
 50.0 µm/m-°C
@Temperature 23.0 - 100 °C
27.8 µin/in-°F
@Temperature 73.4 - 212 °F
 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
33.3 µin/in-°F
@Temperature 73.4 - 302 °F
 100 µm/m-°C
@Temperature >=150 °C
55.6 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 0.303 W/m-K2.10 BTU-in/hr-ft²-°F
Melting Point 280 °C536 °FASTM D3418
Maximum Service Temperature, Air 221 °C430 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 116 °C240 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS); Molded
Mitsubishi Chemical Advanced Materials Techtron™ PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded
Mitsubishi Chemical Advanced Materials Techtron™ 1000 PPS Extruded Polyphenylene Sulfide
Mitsubishi Chemical Advanced Materials Techtron™ PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers

P1SM36 / 20128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.