MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Torlon® AI-10 PAI, High-temperature adhesion promoter for non-stick coatings
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: Torlon® AI-10 is a polyamideimide (PAI) powder developed for the performance coatings industry. As a liquid polymer solution, the resin is incorporated into the formulation of engineered coatings; often as the principal primer, binder, or high temperature adhesive component. As a powder, the resin is used in specialty composites and unique dry spray applications.

Coatings based on the Torlon® AI-10 polymer yield durable, abrasion resistant, thermally stable films that do not exhibit unwanted thermoplastic properties. The resin has superior resistance to organic solvents and a wide array of other commercial and industrial chemicals. Outstanding tribological characteristics are afforded both by the resin as well as its unparalleled intra-coat adhesion to fluoropolymers. Coatings based on AI-10 polymer have been shown to be cost effective in electrical/electronic, high temperature decorative and corrosion preventative applications.

Magnet wire insulation and protective coatings for printed circuit boards are some of the electrical uses. Industrial applications include primers and decorative topcoats for cookware, appliances and housewares. AI-10 polymer has been combined with fluoropolymers to produce high-performance, low-friction, corrosion-resistant coatings that provide protection to saw blades, gears, carburetor needles and lawn and garden tools. Torlon AI-10 is also used for high-strength, high-temperature adhesives. Excellent bond strengths have been observed with stainless steel, aluminum and titanium alloys and polyimide films.

A special grade (called AI-10 LM) has been developed to reduce the amount of residual methylene dianline (MDA) monomer to below the 1000ppm level specified in hazard communication regulations.

A water soluble analog of AI-10 (called Torlon® AI-30) is also available.

Markets/Uses: Coatings / High Performance Coatings / Abrasion Resistant Coatings; Coatings / High Performance Coatings / Corrosion Resistant Coatings; Coatings / High Performance Coatings / High-Temperature Coatings; Coatings / High Performance Coatings / Primers for Non-Stick Coatings

Applications: Adhesives; Binder; Coating Applications

Features: Abrasion Resistant; Chemical Resistant; Flame Retardant; Good Adhesion; High Heat Resistance

Solubility
Torlon AI-10 resin is supplied as a powder that is readily dissolved in N-methyl pyrrolidone (NMP) and other aprotic solvents. Other organic solvents may be used as diluents to reduce viscosity at lower cost. N-methyl pyrrolidone is hydrophilic, and as such, retains considerable amounts of water. Adding non-polar diluents may be appropriate to aid in the application process and to prevent potential formulation and shelf stability issues.

Pigments and Additives
Pigments and additives can be used with Torlon AI-10 polymer to produce special purpose coating and adhesive formulations. Suitable additives include heat-stable organic and inorganic pigments, fillers and certain epoxy and fluoropolymer copolymers. Due to the inherent color of Torlon AI-10 polymer, care must be taken if white or very pale shades are to be successfully formulated. To prevent the absorption of unwanted moisture, all pigments should be ground in closed milling equipment. Likewise, hydroscopic additives, such as fibers and copolymers, should be dried to appropriate moisture levels prior to being incorporated into the formulation.

Application.
Depending on the aesthetic and performance characteristics required, uniform coatings can be applied by spray, roll, spin or curtain techniques. Usually, dry film thicknesses from 10-20 µm are readily achieved in a single coating pass, with multicoat systems affording the opportunity for additional surface build. Regardless of the method employed, it is essential to assure appropriate preparation of the substrate prior to application of coating. Once complete, application equipment should be purged of coating and cleaned with a true solvent.

Drying/Curing
Coatings based upon Torlon AI-10 resin dry and initiate cure at temperatures as low as 150°C (300°F). However, optimal film properties result after heating for 5 to 20 minutes, depending on the film thickness and the formulation, at 250°C (480°F). In the case of multi-coat systems, an intermediate temperature step at around 200°C (390°F) for 10 minutes may be advisable. For coating formulations employing low solids, a brief flash off period of about 3 to 10 minutes may be recommended prior to initiating cure.

Information provided by Solvay Specialty Polymers.

Vendors: Drake Plastics Ltd. Co. The Torlon Specialist, manufactures & stocks the most complete line of Torlon PAI in machinable rod, plate & Seamless Tube®. Drake works closely with Solvay Specialty Polymers to identify & serve a multitude of new applications. Drake, a lean producer of extruded, injection molded & machined shapes & parts, offers low minimums & quick, economical delivery globally.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 1000 cP
@Temperature 23.0 °C
1000 cP
@Temperature 73.4 °F
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPowder
ProcessingCoating; Solution Processing
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4553 / 280353

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.