MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ITW Insulcast® RTVS 11 Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 11 is a low viscosity, multi-purpose compound, designed for use as a potting, encapsulating, sealing and mold making material. Due to its excellent electrical properties, the RTVS 11 is used extensively is a high voltage potting compound, as well as an encapsulating compound for delicatecircuitry. The RTVS 11 can be used with various curing agents, thus varying pot life, cure time, mix ratios and cure conditions.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/cc
Viscosity 12000 cP12000 cPASTM D1084
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ASTM D2240
Tensile Strength 3.45 MPa500 psiASTM D412
Elongation at Break 150 %150 %ASTM D412
Tear Strength 3.51 kN/m20.0 pliDie B; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.00e+14 ohm-cm9.00e+14 ohm-cmASTM D257
Dielectric Constant 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 250 µm/m-°C139 µin/in-°F
Thermal Conductivity 0.0259 W/m-K0.180 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
Shrinkage 0.20 - 0.50 %0.20 - 0.50 %
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
USING 0.3% CAT 2 (DBT). Faster tack-free surfaces achieved using varied catalysts.
Pot Life 15.0 - 120 min15.0 - 120 minvaries with % of CAT-2
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Colorwhite
Mix Ratio by weight0.1 to 0.5%CAT 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Geniomer® 60 Silicone TPE
Multibase TPSiV® 3111-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3011-50A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3010-50A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 1180-50D Thermoplastic Silicone Vulcanizate

PITWIN9115 / 239625

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.