MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kolon KOCETAL® GF302 G/F Reinforced Acetal Resin
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 10% Glass Fiber Reinforced

Material Notes: Glass fiber reinforced, improved stiffness.

Applications: Products for high stiffness, improved fatigue properties.

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
Ash 8.0 - 12 %8.0 - 12 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
Tensile Strength 94.0 MPa13600 psiASTM D638
Elongation at Break 10.3 %10.3 %ASTM D638
Flexural Strength 142 MPa20600 psiASTM D790
Flexural Modulus 4.745 GPa688.2 ksiASTM D790
Izod Impact, Notched 0.430 J/cm0.806 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °FASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Azoty Tarnow™ TARNOFORM 500 GF6 POM
Azoty Tarnow™ TARNOFORM 300 GF7 POM
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM
Celanese Celcon® LW90F5 Tetrafluoroethylene Filled Acetal Copolymer
Celanese Celcon® GC25TF POM, 25% Glass Reinforced

PKOKZ911 / 122613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.