System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Americas Styrenics PolyRenew® 5001 HE High Heat Crystal Polystyrene
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Polystyrene, Heat Resistant Grade
Material Notes:
Product Characteristics
High heat resistance
High tensile strength
Blue tint
Food Contact Compliant
Typical Applications
Foam
OPS
Information provided by AmericasStyrenics LLC.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.04
g/cc
1.04
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0080
cm/cm
0.0040
-
0.0080
in/in
ASTM D955
Melt Flow
1.2
g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.2
g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell L
107
107
ASTM D785
Tensile Strength at Break
51.7
MPa
7500
psi
ASTM D638
Tensile Strength
52.4
MPa
7600
psi
ASTM D638
Elongation at Break
3.0 %
3.0 %
ASTM D638
Tensile Modulus
3.17
GPa
460
ksi
ASTM D638
Flexural Strength
89.6
MPa
13000
psi
ASTM D790
Flexural Modulus
3.24
GPa
470
ksi
ASTM D790
Izod Impact, Notched
0.214
J/cm
0.400
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
CTE, linear
90.0
µm/m-°C
50.0
µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
98.3
°C
209
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
88.9
°C
192
°F
ASTM D648
Vicat Softening Point
108
°C
227
°F
ASTM D1525
Processing Properties
Metric
English
Comments
Processing Temperature
66.0
-
104
°C
151
-
219
°F
Polish Rolls, Extrusion
204
-
221
°C
399
-
430
°F
Zone 6, Extrusion
193
-
232
°C
379
-
450
°F
Melt Pump, Adapter, Pipes, Screen Changer, Extrusion
Nozzle Temperature
230
-
245
°C
446
-
473
°F
Injection
Zone 1
177
-
193
°C
351
-
379
°F
Extrusion
230
-
245
°C
446
-
473
°F
Injection
Zone 2
182
-
204
°C
360
-
399
°F
Extrusion
215
-
230
°C
419
-
446
°F
Injection
Zone 3
188
-
210
°C
370
-
410
°F
Extrusion
200
-
215
°C
392
-
419
°F
Injection
Zone 4
199
-
216
°C
390
-
421
°F
Extrusion
Zone 5
204
-
221
°C
399
-
430
°F
Extrusion
Die Temperature
199
-
232
°C
390
-
450
°F
Extrusion
Melt Temperature
193
-
232
°C
379
-
450
°F
Extrusion
Back Pressure
0.172
-
1.48
MPa
25.0
-
215
psi
Injection
Descriptive Properties
Head Pressure
10-21 MPa
Extrusion
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PAMERI905b / 249346
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.