MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MOL Group TIPELIN 5700S HDPE, Fiber grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); HDPE, Fiber Grade

Material Notes: Description: TIPELIN 5700S is a high density unimodal polyethylene copolymer (with buthene-1 as comonomer) intended for fiber extrusion. It has medium molecular weight and a narrow molecular weight distribution. It offers high tensile strength, high elongation at break and low tendency to fibrillation. The grade contains antioxidant and acid scavenger.

Applications: TIPELIN 5700S is recommended for making split film and tapes, round bale nets and protective netting in agriculture and building industry. Recommended film thickness (Primer film) is 0.06 - 0.12 mm. Recommended film thickness (Fiber) is 0.018 - 0.025 mm.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements on film (MD = machine direction, TD = trans direction) thickness of 0.015 mm, blow up ratio 4:1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.947 g/cc0.0342 lb/in³1; ISO 1183-1
Oxidative Induction Time (OIT) 100 min
@Temperature 200 °C
100 min
@Temperature 392 °F
EN 728
Melt Flow  0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 1.7 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.7 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
25 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62621; ISO 868
Film Tensile Strength at Yield, MD 23.0 MPa3340 psi2; ISO 527-3
Film Tensile Strength at Yield, TD 20.0 MPa2900 psi2; ISO 527-3
Film Elongation at Break, MD 750 %750 %2; ISO 527-3
Film Elongation at Break, TD 900 %900 %2; ISO 527-3
Flexural Modulus 1.20 GPa174 ksi1; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²1; ISO 180/A
Impact 34342, Spencer; ASTM D 3420
Elmendorf Tear Strength MD 17 g17 g2; ISO 6383-2
Elmendorf Tear Strength TD 150 g150 g2; ISO 6383-2
Dart Drop Test 47.0 g0.104 lb2, F50; ISO 7765-1 method A
Film Tensile Strength at Break, MD 46.0 MPa6670 psi2; ISO 527-3
Film Tensile Strength at Break, TD 49.0 MPa7110 psi2; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °F1; ISO 306/A 120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG038 / 297204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.