MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Parabeam Industrie Paraglass 8 3D Glass Fabric
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Core Material; Composite Fibers

Material Notes: Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the decklayers thus forming an integral sandwich structure.
When the Parabeam® is impregnated with a thermoset resin, the fabric absorbs the resin and due to the capillary forces of the piles, the fabric rises to the preset height.
In this one-step process a lightweight and strong sandwich laminate is formed that offers excellent mechanical properties. Parabeam® can be used for many applications in the composite industry while offering multiple advantages against traditional sandwiches and solid laminates such as woods, foams, balsa, honeycombs and more.

Information provided by the manufacturer, Parabeam Industrie, The Netherlands.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 2.00 MPa>= 290 psiASTM C365
 2.70 MPa392 psiASTM C365
Shear Modulus >= 0.0103 GPa>= 1.49 ksiASTM C273
 0.0134 GPa1.94 ksiTypical; ASTM C273
Shear Strength >= 0.300 MPa>= 43.5 psiASTM C273
 0.500 MPa72.5 psiTypical; ASTM C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0600 W/m-K0.416 BTU-in/hr-ft²-°FDIN 52616

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
Parabeam Industrie Paraglass 10 3D Glass Fabric
S-2 Glass® Fiber
Parabeam Industrie Paraglass 3 3D Glass Fabric
AR-Glass Fiber, Generic

CPB3D030 / 1696

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.