MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® HHM TR-144 Polyethylene, Film Grade; HDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: FDA approved.

Data provided by the manufacturer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.947 g/cc0.0342 lb/in³ASTM D1505
Moisture Vapor Transmission 0.200 cc-mm/m²-24hr-atm0.508 cc-mil/100 in²-24hr-atmASTM E96
Oxygen Transmission 59.0 cc-mm/m²-24hr-atm150 cc-mil/100 in²-24hr-atmASTM D1434
Thickness 25.4 microns1.00 mil
Melt Flow 0.18 g/10 min0.18 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 24.0 MPa3480 psiBlown film; ASTM D638
Film Tensile Strength at Yield, TD 26.0 MPa3770 psiBlown film; ASTM D638
Film Elongation at Break, MD 480 %480 %Blown film; ASTM D638
Film Elongation at Break, TD 640 %640 %Blown film; ASTM D638
Flexural Modulus 1.103 GPa160.0 ksiASTM D790
Elmendorf Tear Strength MD 23 g23 gBlown Film; ASTM D1922
Elmendorf Tear Strength TD 330 g330 gBlown Film; ASTM D1922
Elmendorf Tear Strength, MD 0.906 g/micron23.0 g/mil1 mil; Blown Film; ASTM D1922
Elmendorf Tear Strength, TD 13.0 g/micron330 g/mil1 mil; Blown Film; ASTM D1922
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.33
@Frequency 100000 Hz
2.33
@Frequency 100000 Hz
ASTM D1531
Dielectric Strength 20.0 kV/mm
@Thickness 3.17 mm
508 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor >= 0.00010
@Frequency 100000 Hz
>= 0.00010
@Frequency 100000 Hz
ASTM D1531
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 216 °C379 - 421 °FStock Temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reliance Industries Relene E52009 Polyethylene
Versalis Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow HDPE 12450N High Density Polyethylene
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade

PEHM36 / 35507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.