MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylic (PMMA); Acrylonitrile-Methyl Acrylate Copolymer

Material Notes: Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Apparent Bulk Density 0.670 g/cc0.0242 lb/in³
Moisture Vapor Transmission 3.00 cc-mm/m²-24hr-atm7.62 cc-mil/100 in²-24hr-atm
Oxygen Transmission 0.600 cc-mm/m²-24hr-atm1.52 cc-mil/100 in²-24hr-atm
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/inASTM D955
Melt Flow 3.0 g/10 min
@Load 12.5 kg,
Temperature 200 °C
3.0 g/10 min
@Load 27.6 lb,
Temperature 392 °F
2 mm x 8 mm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060
Hardness, Rockwell R 115115
Hardness, Shore D 8686
Tensile Strength, Yield 65.0 MPa9430 psi
Elongation at Break 3.0 %3.0 %
Flexural Yield Strength 95.0 MPa13800 psi
Flexural Modulus 3.40 GPa493 ksi
Compressive Yield Strength 83.0 MPa12000 psi
Izod Impact, Notched 5.00 J/cm9.37 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.90e+15 ohm-cm1.90e+15 ohm-cm
Surface Resistance >= 2.00e+17 ohm>= 2.00e+17 ohm
Dielectric Constant 5.2
@Frequency 100 Hz
5.2
@Frequency 100 Hz
Dissipation Factor 0.070
@Frequency 100 Hz
0.070
@Frequency 100 Hz
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.80 J/g-°C0.430 BTU/lb-°F
Thermal Conductivity 0.690 W/m-K4.79 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C171 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FASTM D648
Vicat Softening Point 83.0 °C181 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5111.511
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer
Overview of materials for PVC/Acrylic Alloy
Trinseo Plexiglas® V825 Acrylic
Trinseo Solarkote™ A200 Acrylic
Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin

PABSB0 / 22113

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.