System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Zytel® HTNFG52G35HSL BK011 PA6T/66-GF35
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6/66
;
Nylon 66/6, 40% Glass Fiber Reinforced
Material Notes:
35% Glass Reinforced, PPA, High Performance Polyamide
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.45
g/cc
0.0524
lb/in³
DAM; ISO 1183
Melt Density
1.10
g/cc
@Temperature 325 °C
0.0397
lb/in³
@Temperature 617 °F
Water Absorption
0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
Immersion; DS; DAM; Sim. to ISO 62
Moisture Absorption
2.00 %
@Thickness 2.00 mm
2.00 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0020
cm/cm
0.0020
in/in
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
0.0080
in/in
DAM; ISO 294-4, 2577
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
180
MPa
26100
psi
50% RH; ISO 527-1/-2
200
MPa
29000
psi
DAM; ISO 527-1/-2
Elongation at Break
1.8 %
1.8 %
DAM; ISO 527-1/-2
2.2 %
2.2 %
50% RH; ISO 527-1/-2
Tensile Modulus
12.0
GPa
1740
ksi
50% RH; ISO 527-1/-2
12.0
GPa
1740
ksi
DAM; ISO 527-1/-2
Poissons Ratio
0.33
0.33
50% RH
0.33
0.33
DAM
Charpy Impact Unnotched
3.80
J/cm²
@Temperature 23.0 °C
18.1
ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
3.80
J/cm²
@Temperature 23.0 °C
18.1
ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched
0.800
J/cm²
@Temperature 23.0 °C
3.81
ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
0.800
J/cm²
@Temperature 23.0 °C
3.81
ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
DAM; IEC 62631-3-1
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
20.0
µm/m-°C
11.1
µin/in-°F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow
60.0
µm/m-°C
33.3
µin/in-°F
DAM; ISO 11359-1/-2
Melting Point
310
°C
590
°F
first heat; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)
285
°C
545
°F
DAM; ISO 75-1/-2
Glass Transition Temp, Tg
45.0
°C
113
°F
10°C/min; 50% RH; ISO 11357-1/-2
90.0
°C
194
°F
10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
DAM; IEC 60695-11-10
HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread
<=
80.0
mm/min
@Thickness 1.00 mm
<=
3.15
in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index
25 %
25 %
DAM; ISO 4589-1/-2
Processing Properties
Metric
English
Comments
Melt Temperature
325
°C
617
°F
Optimum, Injection
320
-
330
°C
608
-
626
°F
Range, Injection
Mold Temperature
90.0
-
110
°C
194
-
230
°F
Injection
Drying Temperature
100
°C
212
°F
Injection
Dry Time
6.00
-
8.00
hour
6.00
-
8.00
hour
Injection, Dehumidified Dryer
Moisture Content
<= 0.10 %
<= 0.10 %
Injection
Descriptive Properties
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
ISO designation
ISO 16396-PA6T/66,GF35,M1CGHR,S10-120
Part Marking Code
>PA6T/66-GF35<
ISO 11469
>PPA-GF35<
SAE J1344
Polymer
PA6T/66-GF35
Resin Identification
PA6T/66-GF35
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced
Celanese Celstran® PA66-GF40-0101P10/11 PA666, 40% Glass Reinforced
Akro-Plastic Akromid® C3 GF 40 1 (4658) PA66/6 Dry, 40% Glass Filled
Celanese Zytel® HTN52G45HSL BK083 PA6T/66-GF45
Celanese Zytel® HTN52G35HSL BK083 PA6T/66-GF35
PDSX5459 / 198099
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.