MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.

Applications: External door handles in vehicles, visible sunroof frames, over door handles, toaster castings, external mirrors, rear screen wiper arms in vehicles and sunroof wind deflectors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³ISO 1183
Water Absorption 0.40 %0.40 %DIN 53495/1L
Moisture Absorption at Equilibrium 0.12 %0.12 %23°C/50% R.H.
Viscosity Number 90 cm³/g0.90 dl/g
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inSheet
 0.0024 cm/cm0.0024 in/in60x60x2mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0075 cm/cm0.0075 in/inSheet
 0.0077 cm/cm0.0077 in/in60x60x2mm; ISO 294
Melt Flow 10.4 g/10 min
@Load 2.16 kg,
Temperature 275 °C
10.4 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psi5mm/min; ISO 527-2
Elongation at Break 1.5 %1.5 %5mm/min; ISO 527-2
Modulus of Elasticity 18.7 GPa2710 ksiISO 527-2
Charpy Impact Unnotched 5.20 J/cm²24.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
Dart Drop, Total Energy <= 5.00 J<= 3.69 ft-lbISO 6603-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmIEC 60093
Dielectric Constant  4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
IEC 60250
 4.7
@Frequency 100 Hz
4.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm406 kV/inIEC 243/1
Dissipation Factor  0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 225 V225 VTest solution A; IEC 112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.60 J/g-°C0.382 BTU/lb-°FIEC 1006
Melting Point 220 - 250 °C428 - 482 °F
Maximum Service Temperature, Air 140 °C284 °Fat 50% loss of tensile strength after 20000h; IEC 216-1
 160 °C320 °Fat 50% loss of tensile strength after 5000h; IEC 216-1
 210 °C410 °F
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection molding
 270 °C518 °Ffor shrinkage test
Mold Temperature 60.0 - 100 °C140 - 212 °F
 80.0 °C176 °Ffor shrinkage test
 
Descriptive Properties
ColorBK5110 and Colored
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicRelease agent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
BASF Ultradur® B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
BASF Ultradur® B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
BASF Ultradur® B 4300 G4 BK5110 20% Glass Filled PBT

PBASF9058 / 84822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.