MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toray TORAYCA™ VX84K-20 PBT/ABS, CF + GF
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Short carbon fiber reinforced PBT, CF+GF, Flame retardant, PBT+ABS(CF+GF)20FR(17).

General Torayca™ Notes: TORAYCA™ is a carbon fiber reinforced thermoplastic (CFRTP) that is light weight and features excellent strength, stiffness, dimensional accuracy, and sliding properties. Physical property: Carbon fiber reinforced thermoplastic (CFRTP) offer excellent mechanical strength/rigidity and maintain a combination of characteristics. Lower specific gravity and lightweight, High creep resistance and fatigue resistance, Excellent abrasion resistance and sliding properties. Low molding shrinkage and coefficient of linear expansion, ensuring high dimensional accuracy, Excellent electrical conductivity and electromagnetic shielding performance.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.395 g/cc0.05040 lb/in³ISO 1183
Filler Content 20 %20 %
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in80x80x3mmt.; Toray Method
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in80x80x3mmt.; Toray Method
Melt Flow 40 g/10 min40 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 145 MPa
@Temperature 23.0 °C
21000 psi
@Temperature 73.4 °F
ISO 527-1,2
Elongation at Break 2.7 %
@Temperature 23.0 °C
2.7 %
@Temperature 73.4 °F
ISO 527-1,2
Flexural Strength 220 MPa
@Temperature 23.0 °C
31900 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 13.0 GPa
@Temperature 23.0 °C
1890 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
V-Notched; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 171 °C340 °FISO 75-1,2
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9170 / 248859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.