MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Available in unlimited lengths - no seams in finished products.

Data provided by the manufacturer, Plaskolite, Inc.

Key Words: PMMA; Polymethyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6868Method A; ASTM D785
Tensile Strength, Yield 55.0 MPa7980 psiASTM D638
Tensile Modulus 2.30 GPa334 ksiASTM D638
Flexural Yield Strength 83.0 MPa12000 psiASTM D790
Izod Impact, Notched 0.700 J/cm1.31 ft-lb/inASTM D256
 0.200 J/cm
@Temperature -18.0 °C
0.375 ft-lb/in
@Temperature -0.400 °F
ASTM D256
Gardner Impact 3.70 J2.73 ft-lbreported as J/cm; ASTM D3029-GB, unpainted
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F
@Temperature -0.400 - 100 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °Fannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Transmission, Visible 92 %92 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 157 °C315 °FOptimal Thermoforming temperature for sheet 0.25-1.0 cm (0.10-0.39 in)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Acrylic, Optical Grade, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified
Plaskolite Optix® PL-52 Acrylic Resin

PPLASC / 56285

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.