MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PA 66 Technical plastic
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: PA 66 differs from PA 6 due to its higher strength, rigidity, temperature resistance, and wear resistance as well as improved creep resistance. However, it has lower impact toughness and mechanical damping behavior.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³DIN EN ISO 1183-1
Moisture Absorption 2.80 %2.80 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383DIN EN ISO 868
Ball Indentation Hardness 180 MPa26100 psiDIN EN ISO 2039-1
Tensile Strength, Yield 85.0 MPa12300 psi50 mm/min; DIN EN ISO 527
Elongation at Break 50 %50 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 3.30 GPa479 ksi1 mm/min; DIN EN ISO 527
Charpy Impact, Notched >= 0.300 J/cm²>= 1.43 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.83.8IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243
Dielectric Loss Index 0.0150.015IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
DIN 53752
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°F
Melting Point 260 °C500 °FISO 11357-3
Maximum Service Temperature, Air 95.0 °C203 °Fshort term
 170 °C338 °Flong term
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FDIN EN ISO 75/A
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 V-2
@Thickness 6.00 mm
V-2
@Thickness 0.236 in
 
Descriptive Properties
Colornatural (cream), black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP025 / 250523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.