MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema EVATANE® 24-03 Copolymer Ethylene - Vinyl Acetate
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: EVATANE® 24-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 24-03 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 24-03 brings softness, flexibility and polarity. EVATANE® 24-03 delivers high cohesive strength with any kind of fillers (masterbatchs, HFFR compounds). EVATANE® 24-03 is also very well adapted for the production of cast or blown films. It can also be used as an additive for bitumen.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc
@Temperature 23.0 °C
0.0340 lb/in³
@Temperature 73.4 °F
ISO 1183
Vinyl Acetate Content 23 - 25 %23 - 25 %FTIR (internal)
Melt Index of Compound 2.5 - 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 - 3.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D2240
Tensile Strength at Break 27.0 MPa3920 psiASTM D638
Elongation at Break 600 - 900 %600 - 900 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 °C176 °FDSC
Vicat Softening Point 46.0 °C
@Load 0.999 kg
115 °F
@Load 2.20 lb
ISO 306
Ring & Ball Softening Point 183 °C361 °FASTM E28
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 230 °C<= 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate
Arkema EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
Arkema EVATANE® 18-500 Copolymer Ethylene - Vinyl Acetate
Arkema EVATANE® 18-150 Copolymer Ethylene - Vinyl Acetate

PARKG076 / 80132

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.