MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shakespeare Resistat® F9222 B040 Nylon 6 Monofilament
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6 Fiber

Material Notes: Resistat F9222, MERGE B040 is a 22 denier per filament conductive nylon 6 tow. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating thickness of approximately 1 micron. It is available with a 40 filaments version yielding a total of 915 denier. The yarn color is black. Resistat is used for carpeting, ESD garments, and industrial belting and brushes.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Fiber Count 1020 dtex915 denier
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 15 %15 %
Tenacity 0.265 N/tex3.00 g/denier
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 4000 ohm-cm4000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 °C419 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NYCOA 870 PA 6
Nurel Engineering Polymers Promyde® B26 C PA 6
Envalior Akulon® F-X9182 PA6
BASF Ultramid® B27 SD 05 PA6
BASF Ultramid® B27 E 01 PA6 (Dry)

PSHAKE020 / 67299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.