MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Rynite® FR533NH NC010 PET-GF33FR(40)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: 33% Glass Reinforced, Flame Retardant, Non-Halogenated, Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psiISO 527-1/-2
Elongation at Break 0.90 %0.90 %ISO 527-1/-2
Tensile Modulus 13.1 GPa1900 ksiISO 527-1/-2
Flexural Strength 143 MPa20700 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Poissons Ratio 0.330.33
Charpy Impact, Notched  1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243-1
Comparative Tracking Index 350 V350 VIEC 60112
 250 - 399 V
@Thickness 3.00 mm
250 - 399 V
@Thickness 0.118 in
PLC 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FISO 11359-1/-2
 11.0 µm/m-°C
@Temperature 55.0 - 160 °C
6.11 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
 18.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
10.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 72.0 µm/m-°C40.0 µin/in-°FISO 11359-1/-2
 51.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
28.3 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 81.0 µm/m-°C
@Temperature 55.0 - 160 °C
45.0 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
Melting Point 249 °C480 °F10°C/min; ISO 11357-1/-3
Hot Ball Pressure Test 230 °C446 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75-1/-2
Glass Transition Temp, Tg 90.0 °C194 °F10°C/min; ISO 11357-1/-2
UL RTI, Electrical  155 °C
@Thickness 0.400 mm
311 °F
@Thickness 0.0157 in
UL 746B
 155 °C
@Thickness 0.750 mm
311 °F
@Thickness 0.0295 in
UL 746B
 155 °C
@Thickness 1.50 mm
311 °F
@Thickness 0.0591 in
UL 746B
 155 °C
@Thickness 3.00 mm
311 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
IEC 60695-11-10
 5VA
@Thickness 0.750 mm
5VA
@Thickness 0.0295 in
IEC 60695-11-20
Glow Wire Ignition Temperature  775 °C
@Thickness 1.50 mm
1430 °F
@Thickness 0.0591 in
IEC 60695-2-13
 825 °C
@Thickness 0.750 mm
1520 °F
@Thickness 0.0295 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 280 °C518 - 536 °FRange, Injection
 280 °C536 °FOptimum, Injection
Mold Temperature 120 - 140 °C248 - 284 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
 
Descriptive Properties
AdditivesFlame retardant
 Non-halogenated/Red phosphorous free flame retardant
Drying RecommendedyesInjection
Part Marking Code>PET-GF33FR(40)<ISO 11469
PolymerPET-GF33 FR(40)
Railway classificationR22DIN 53236
Railway classification ratingHL1EN 45545-2
Resin IdentificationPET-GF33FR(40)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled
Celanese Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)
BASF Petra® 330 FR BK-112 30% Glass Filled PET
BASF Petra® 130 FR 30% Glass Filled PET
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6

PDSX5276 / 197916

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.