MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 1-0889-4 Polyamide 66 with carbon fiber and glass fiber, heat stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Material Notes: Properties/attributes include: Strong, stiff parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Reduced moment of inertia compared with metal parts.

Automotive industry, textile- and office machinery, apparatus- and precision engineering.

Processing: During processing the moisture level should not exceed 0.1%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Excessively high predrying temperatures may cause discoloration. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccISO 1183
Moisture Absorption <= 1.00 %
@Temperature 23.0 °C,
Time 86400 sec
<= 1.00 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 205 MPa29700 psiISO 527-2
Elongation at Break 3.0 %3.0 %ISO 527-2
Modulus of Elasticity 13.0 GPa1890 ksiISO 527-2
Flexural Strength 290 MPa42100 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Flexural Strain at Break 3.9 %3.9 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 10000 ohm-cm<= 10000 ohm-cmIEC 60167
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °FContinuous; UL 746B
 160 °C320 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °F
Zone 1 290 - 310 °C554 - 590 °F
Zone 2 290 - 310 °C554 - 590 °F
Zone 3 290 - 310 °C554 - 590 °F
Melt Temperature 290 °C554 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature  75.0 °C
@Time 21600 - 57600 sec
167 °F
@Time 6.00 - 16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 21600 sec
221 °F
@Time 4.00 - 6.00 hour
Vacuum Dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1-0889-2 Polyamide 66 with carbon fiber and glass fiber, heat stabilized

PLUU8813 / 193772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.