Forms: Pellets
Filler/Reinforcement: Glass/Stainless Steel Fiber
Additive: Lubricated
Features: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequency Shielding (RFI)
Appearance: Blue