MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Injection Molding, High rigidity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 220 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 26.0 MPa3770 psi50 mm/min, 4 mm; ISO 527
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min, 4 mm; ISO 527
Elongation at Break 25 %25 %50 mm/min, 4mm; ISO 527
Elongation at Yield 2.0 %2.0 %50 mm/min, 4mm; ISO 527
Flexural Strength 51.0 MPa7400 psi2 mm/min, 4 mm; ISO 178
Flexural Modulus 2.20 GPa319 ksi2 mm/min, 4 mm; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 11.0 J/cm²52.4 ft-lb/in²ISO 179
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °Funannealed; ISO 75
 83.0 °C181 °Fannealed; ISO 75
Vicat Softening Point  76.0 °C
@Load 5.00 kg
169 °F
@Load 11.0 lb
50°C/hr; ISO 306
 81.0 °C
@Load 5.00 kg
178 °F
@Load 11.0 lb
120°C/hr; ISO 306
 96.0 °C
@Load 1.00 kg
205 °F
@Load 2.20 lb
50°C/hr; ISO 306
 99.0 °C
@Load 1.00 kg
210 °F
@Load 2.20 lb
120°C/hr; ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1192 A (SBS) Liner Block Copolymer
Chi Mei Kibiton® PB-511 SBC
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer
Chi Mei Kibiton® PB-5903 SBC
Chi Mei Kibiton® PB-585R SBC

PCHI982 / 109470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.