MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Superplastic Zinc (Zn-22Al), Rolled and Annealed
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Annealing Temperature 315°C; Air-Cooled

Properties vary with rolling direction. Values for longitudinal and transverse directions are listed separately.

Key Words: Super Z300; Formetal 22 Alloy; Korloy 2684
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.20 g/cc0.188 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 84 - 8584 - 85500 kg load; 10 mm hardened steel ball
Hardness, Knoop 109109Estimated from Brinell Value
Hardness, Rockwell A 36.536.5Estimated from Brinell Value
Hardness, Rockwell B 52.652.6Estimated from Brinell Value
Hardness, Vickers 9696Estimated from Brinell Value
Tensile Strength, Ultimate 400 - 441 MPa58000 - 64000 psi
Tensile Strength, Yield 370 MPa
@Strain 0.2 %
53700 psi
@Strain 0.2 %
Modulus of Elasticity 68.0 - 93.0 GPa9860 - 13500 ksi
Impact Test 9.49 - 27.1 J
@Temperature 20.0 °C
7.00 - 20.0 ft-lb
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000600 ohm-cm0.00000600 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 26.6 - 26.8 µm/m-°C
@Temperature 20.0 °C
14.8 - 14.9 µin/in-°F
@Temperature 68.0 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 250 - 270 °C482 - 518 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 21 - 23 %21 - 23 %
Cadmium, Cd <= 0.010 %<= 0.010 %
Copper, Cu 0.40 - 0.60 %0.40 - 0.60 %
Iron, Fe <= 0.0020 %<= 0.0020 %
Lead, Pb <= 0.010 %<= 0.010 %
Magnesium, Mg 0.0080 - 0.012 %0.0080 - 0.012 %
Tin, Sn <= 0.0010 %<= 0.0010 %
Zinc, Zn 76.365 - 78.592 %76.365 - 78.592 %As balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Superplastic Zinc (Zn-22Al), Rolled and Annealed - Longitudinal Properties
Superplastic Zinc (Zn-22Al), As-Rolled
Superplastic Zinc (Zn-22Al), As-Rolled - Longitudinal Properties
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Sand Cast
Overview of materials for Zinc Alloy

MZN745 / 14559

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.