MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

API Megol AM T A SEBS Adhesion Modified Overmolding for Polar Polymers
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as there are no VOC emissions from adhesives and, as the components are not made from a range of incompatible materials, they are more easily recycled at the end of their useful life. The over-molding process can be used in highly technical applications such as components for the automotive industry, shells and casings for power tools, parts for domestic appliances, and seals which can be molded directly onto the frame.

Information provided by A.P.I. SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 - 0.890 g/cc0.0318 - 0.0322 lb/in³ASTM D 638
 0.890 g/cc0.0322 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  60
@Time 15.0 sec
60
@Time 0.00417 hour
Median; ASTM D 2240
 40 - 80
@Time 54000 sec
40 - 80
@Time 15.0 hour
ASTM D 2240
Tensile Strength 0.588 - 0.706 MPa85.3 - 102 psiASTM D 638
 6.70 MPa972 psiMedian; ASTM D 638
Elongation at Break 550 - 700 %550 - 700 %ASTM D 638
 650 %650 %Median; ASTM D 638
100% Modulus  0.108 - 0.412 MPa
@Strain 100 %
15.6 - 59.7 psi
@Strain 100 %
ASTM D 638
 2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
Median; ASTM D 638
300% Modulus  1.90 - 5.00 MPa
@Strain 300 %
276 - 725 psi
@Strain 300 %
ASTM D 638
 3.50 MPa
@Strain 300 %
508 psi
@Strain 300 %
Median; ASTM D 638
Tear Strength 32.0 kN/m183 pliMedian; ASTM D 624
 21.6 - 43.1 kN/m123 - 246 pliASTM D 624
 
Descriptive Properties
CompatibilityEVA
 PE
 PP
Food ContactOk
IgroscopicityNo
Main FeaturesTranslucent
Ozone Aging ResistanceExcellent72h, 40°C, 200 ppcm, Tension = 20%
ProcessingInjection Molding
WeatheringExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Alcryn® 2060 NC Melt Processable Rubber
A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
A. Schulman Alcryn® 2170 BK Melt Processable Rubber
A. Schulman Alcryn® 2160 BK Melt Processable Rubber

PAPISp908 / 170652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.