MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubriplate SYNCOOL 32 Polyglycolester-Based Synthetic Air Compressor Fluid
Categories: Fluid; Lubricant; Polyglycol

Material Notes: These polyglycolester-based synthetic fluids are designed for rotary screw air compressors. They offer excellent heat transfer properties, low evaporation, high flash points, and outstanding oxidation resistance, eliminating varnish and sludge. Fluid change intervals are 8,000 hours under normal operating conditions.

Syncool Series Fluids are available in Pails & Drums.

Information provided by Lubriplate

Key Words: Part Number L0965-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 3232ISO Grade
 156156Viscosity Index
Saybolt Viscosity at 100°F 165 SUS165 SUS
Saybolt Viscosity at 210°F 34 SUS34 SUS
Kinematic Viscosity at 40°C (104°F) 30 cSt30 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt6.0 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -51.1 °C-60.0 °F
Flammability Test 550550[°F] Fire Point
Flash Point 252 °C485 °F
 
Descriptive Properties
SAE No.10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WLUBR012 / 76058

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.