MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Very Low Density Polyethylene (VLDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Very Low Density Polyethylene (VLDPE)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.887 - 0.923 g/cc0.0320 - 0.0333 lb/in³Average value: 0.909 g/cc Grade Count:24
Moisture Vapor Transmission 0.0300 - 0.0714 cc-mm/m²-24hr-atm0.0762 - 0.181 cc-mil/100 in²-24hr-atmAverage value: 0.0438 cc-mm/m²-24hr-atm Grade Count:3
Thickness 8.00 - 51.0 microns0.315 - 2.01 milAverage value: 30.8 microns Grade Count:17
Melt Flow 0.770 - 13.0 g/10 min0.770 - 13.0 g/10 minAverage value: 2.96 g/10 min Grade Count:24
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 26.0 - 40.026.0 - 40.0Average value: 31.3 Grade Count:3
Tensile Strength, Ultimate 9.00 - 15.0 MPa1310 - 2180 psiAverage value: 12.3 MPa Grade Count:3
Film Tensile Strength at Yield, MD 5.00 - 68.3 MPa725 - 9910 psiAverage value: 12.0 MPa Grade Count:12
Film Tensile Strength at Yield, TD 5.00 - 66.9 MPa725 - 9700 psiAverage value: 11.6 MPa Grade Count:12
Tensile Strength, Yield 4.00 - 8.00 MPa580 - 1160 psiAverage value: 5.67 MPa Grade Count:3
Film Elongation at Break, MD 400 - 800 %400 - 800 %Average value: 555 % Grade Count:13
Film Elongation at Break, TD 590 - 1000 %590 - 1000 %Average value: 798 % Grade Count:12
Elongation at Break 700 - 750 %700 - 750 %Average value: 733 % Grade Count:3
Flexural Modulus 0.0450 - 0.115 GPa6.53 - 16.7 ksiAverage value: 0.0733 GPa Grade Count:3
Secant Modulus, MD 0.0400 - 0.231 GPa5.80 - 33.5 ksiAverage value: 0.104 GPa Grade Count:9
Secant Modulus, TD 0.0500 - 0.241 GPa7.25 - 34.9 ksiAverage value: 0.114 GPa Grade Count:9
Puncture Energy 1.76 - 5.84 J1.30 - 4.31 ft-lbAverage value: 4.08 J Grade Count:3
Coefficient of Friction 0.140 - 1.000.140 - 1.00Average value: 0.498 Grade Count:9
Elmendorf Tear Strength MD 120 - 710 g120 - 710 gAverage value: 458 g Grade Count:13
Elmendorf Tear Strength TD 499 - 1030 g499 - 1030 gAverage value: 700 g Grade Count:13
Elmendorf Tear Strength, MD 3.57 - 17.7 g/micron90.6 - 450 g/milAverage value: 12.2 g/micron Grade Count:18
Elmendorf Tear Strength, TD 8.36 - 25.6 g/micron212 - 650 g/milAverage value: 19.4 g/micron Grade Count:18
Dart Drop 6.00 - 33.2 g/micron152 - 843 g/milAverage value: 22.2 g/micron Grade Count:15
Dart Drop Test 120 - 1000 g0.265 - 2.20 lbAverage value: 314 g Grade Count:6
Film Tensile Strength at Break, MD 13.0 - 76.6 MPa1890 - 11100 psiAverage value: 46.8 MPa Grade Count:13
Film Tensile Strength at Break, TD 20.0 - 63.6 MPa2900 - 9230 psiAverage value: 38.3 MPa Grade Count:12
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 122 °C230 - 252 °FAverage value: 115 °C Grade Count:10
Vicat Softening Point 38.0 - 95.0 °C100 - 203 °FAverage value: 78.6 °C Grade Count:18
Brittleness Temperature -70.0 °C-94.0 °FAverage value: -70.0 °C Grade Count:7
 
Optical PropertiesMetricEnglishComments
Haze 0.600 - 25.0 %0.600 - 25.0 %Average value: 6.19 % Grade Count:16
Gloss 25.0 - 95.0 %25.0 - 95.0 %Average value: 70.2 % Grade Count:12
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:7
 
Processing PropertiesMetricEnglishComments
Processing Temperature 86.0 - 274 °C187 - 525 °FAverage value: 188 °C Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade

O3808 / 78252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.