MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals PF741 PVC Paste Resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: SCG™ PVC PF741 is a high molecular weight homopolymer paste PVC resin, produced by TPC Paste Resin Co., Ltd. under OxyChem’s HYBRID technology.

Applications: Synthetic leather (top layer, foam layer), automotive sealants & mastic.

Features: Good foaming properties and fine cell structure. Give thicker chemically blown foam at high plasticizer content. Exhibits no flow like even at high shear rates. Good viscosity stability. High physical strength. Good heart stability.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.30 %
@Temperature 110 °C
0.30 %
@Temperature 230 °F
ISO-1269
Viscosity 6500 cP
@Temperature 25.0 °C
6500 cP
@Temperature 77.0 °F
Severs Viscosity 2 hours after mixing, DOP 60 phr; RY-W-QC-E030
Brookfield Viscosity 3600 cP
@Temperature 23.0 °C
3600 cP
@Temperature 73.4 °F
20 rpm, 2 hours after mixing, DOP 60phr; ASTM D1824
 
Descriptive Properties
AppearanceWhite powder
Degree of Polymerization1470refer JIS K 6721
K Value74ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC833 / 278090

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.