MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals ICORENE® 1761 Medium density mettallocene polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: ICORENE® 1761 is medium density mettallocene polyethylene for rotational molding. ICORENE® 1761 is suitable for using in general purpose applications. It has a good balance of properties such as toughness, easy flow, high impact, and surface gloss.

Applications: General propose, Molds, Dies, Tools.

Features: Good toughness. Good UV resistance. High flow. High gloss.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³Anneal; ASTM D 1505
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 0.700 GPa102 ksiASTM D790
Dart Drop Total Energy 190 J/cm0.356 ft-lb/milTest based on ISO 6603
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FISO 11357
Vicat Softening Point 121 °C250 °FISO 306
 
Descriptive Properties
AppearanceColored powder
 Natural powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC733 / 277990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.