MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Ryton® XE5515BL PPS Alloy, 15% glass filled for blow molding and extrusion
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Unreinforced, Extruded

Material Notes: 15% glass filled PPS allow for blow molding and extrusion processes; black color

Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusion or blow molding.

Markets/Uses: Automotive / Air Induction / CAC Hot Air Ducts

Applications: Automotive Applications

Features: Chemical Resistant; Good Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Thickness 3.20 mm
0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 12 g/10 min12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 118118ASTM D785
Hardness, Rockwell R 8787ASTM D785
Tensile Strength 103 MPa14900 psiASTM D638
Tensile Stress 110 MPa16000 psiISO 527-2
Elongation at Break 2.9 %2.9 %ASTM D638
 2.9 %2.9 %ISO 527-2
Tensile Modulus 5.80 GPa841 ksiISO 527-2
 6.21 GPa901 ksiASTM D638
Flexural Strength 159 MPa23100 psiASTM D790
 170 MPa24700 psiISO 178
Flexural Modulus 5.50 GPa798 ksiISO 178
 5.52 GPa801 ksiASTM D790
Poissons Ratio 0.410.41ASTM E132
Izod Impact, Notched 0.960 J/cm
@Thickness 3.18 mm
1.80 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.90 J/cm
@Thickness 3.18 mm
12.9 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 45.0 kJ/m²21.4 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D257
Insulation Resistance 1.00e+13 ohm
@Temperature 90.0 °C
1.00e+13 ohm
@Temperature 194 °F
IEC 60167
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150
 3.6
@Frequency 1000 Hz
3.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm610 kV/inASTM D149
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 100 sec100 secASTM D495
Comparative Tracking Index 150 V150 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  20.0 µm/m-°C
@Temperature 100 - 200 °C
11.1 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
 30.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
16.7 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
30.6 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
 90.0 µm/m-°C
@Temperature 100 - 200 °C
50.0 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Oxygen Index 50 %50 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingBlow Molding; Extrusion
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4462 / 280262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.