MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Zinc Sulfide Cleartran (ZnS)
Categories: Ceramic; Sulfide/Chalcogenide; Other Engineering Material; Semiconductor

Material Notes: Optical Crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.09 g/cc
@Temperature 20.0 °C
0.148 lb/in³
@Temperature 68.0 °F
Solubility 0.000065 ppm0.000065 ppm
Molecular Weight 97.43 g/mol97.43 g/mol
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 14.714.7MPa
Modulus of Elasticity 74.5 GPa10800 ksi
Poissons Ratio 0.280.28
Shear Modulus 29.1 GPa4220 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.50 µm/m-°C
@Temperature -60.0 - 60.0 °C
3.61 µin/in-°F
@Temperature -76.0 - 140 °F
Specific Heat Capacity 0.515 J/g-°C0.123 BTU/lb-°F
Thermal Conductivity 27.2 W/m-K
@Temperature 38.0 °C
189 BTU-in/hr-ft²-°F
@Temperature 100 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.200842.20084at n10.0
 2.449152.44915at n0.4678
 2.15252
@Wavelength 13000 nm
2.15252
@Wavelength 13000 nm
 2.24661
@Wavelength 5000 nm
2.24661
@Wavelength 5000 nm
 2.31669
@Wavelength 780 nm
2.31669
@Wavelength 780 nm
 2.48918
@Wavelength 435.8 nm
2.48918
@Wavelength 435.8 nm
Transmission, Visible 60 %
@Wavelength 500 nm
60 %
@Wavelength 500 nm
Internal Transmittance
IR Transmittance  5.0 %
@Wavelength 15000 nm
5.0 %
@Wavelength 15000 nm
Internal Transmittance
 70 %
@Wavelength 10000 nm
70 %
@Wavelength 10000 nm
Internal Transmittance
UV Transmittance 9.0 %
@Wavelength 350 nm
9.0 %
@Wavelength 350 nm
Internal Transmittance
 
Descriptive Properties
Symmetrycubic
Thermal Coefficient of Refractive Index5.43E-05at 0.6328 microns
Transmission Range (microns)0.37 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Germanium, Ge
Schott IRC-1 Zinc Sulfide Broadband Infrared Ceramic
Zinc Selenide, ZnSe
Mateck Zinc Sulphide, ZnS
Zinc Sulfide, ZnS, Sphalerite (Zincblende)

CMAT059 / 87743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.