MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Mineral Filled

Material Notes: Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 - 1.80 g/cc1.50 - 1.80 g/ccIEC 1212-2 7.2
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength >= 100 MPa
@Diameter >=100 mm
>= 14500 psi
@Diameter >=3.94 in
Perpendicular to laminations; IEC 1212-2 4.1
Compressive Strength >= 60.0 MPa>= 8700 psiAxial; IEC 1212-2 4.2
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+8 ohm
@Diameter 8.00 - 10.0 mm
>= 1.00e+8 ohm
@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Dielectric Constant <= 5.2
@Frequency 1e+6 Hz
<= 5.2
@Frequency 1e+6 Hz
IEC 1212-2 5.3
Dielectric Breakdown  >= 30000 V
@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V
@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
 >= 30000 V
@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V
@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Dissipation Factor <= 0.040
@Frequency 1e+6 Hz
<= 0.040
@Frequency 1e+6 Hz
IEC 1212-2 5.3
 
Descriptive Properties
Cohesion between layers> 30 MPaIEC 1212-2 4.3, Internal diameter <100 mm
Thermal Endurance155 T.I.IEC 1212-2 7.1
Water Absorption< 2 mg/cm²IEC 1212-2 7.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Overview of materials for Silicone Rubber
Rogers Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Pyrotek C-1 Ceramic fiber paper
Overview of materials for Liquid Silicone Rubber

PHIPPE941 / 121945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.