MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 610, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.34 g/cc0.0375 - 0.0484 lb/in³Average value: 1.22 g/cc Grade Count:16
Filler Content 15.0 - 40.0 %15.0 - 40.0 %Average value: 27.1 % Grade Count:7
Water Absorption 0.120 - 0.300 %0.120 - 0.300 %Average value: 0.197 % Grade Count:9
Moisture Absorption at Equilibrium 0.170 - 0.600 %0.170 - 0.600 %Average value: 0.457 % Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0160 cm/cm0.00100 - 0.0160 in/inAverage value: 0.00394 cm/cm Grade Count:11
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 31.4 - 234 MPa4560 - 34000 psiAverage value: 163 MPa Grade Count:16
Elongation at Break 1.50 - 10.0 %1.50 - 10.0 %Average value: 4.02 % Grade Count:15
Modulus of Elasticity 2.30 - 27.6 GPa333 - 4000 ksiAverage value: 14.3 GPa Grade Count:14
Flexural Yield Strength 89.6 - 372 MPa13000 - 54000 psiAverage value: 261 MPa Grade Count:13
Flexural Modulus 2.76 - 22.1 GPa400 - 3200 ksiAverage value: 13.8 GPa Grade Count:13
Izod Impact, Notched 0.366 - 1.60 J/cm0.685 - 3.00 ft-lb/inAverage value: 0.984 J/cm Grade Count:11
Izod Impact, Unnotched 4.27 - 10.7 J/cm8.00 - 20.0 ft-lb/inAverage value: 7.61 J/cm Grade Count:8
Izod Impact, Notched (ISO) 18.0 - 30.0 kJ/m²8.57 - 14.3 ft-lb/in²Average value: 26.0 kJ/m² Grade Count:3
 14.0 - 20.0 kJ/m²
@Temperature -30.0 - -30.0 °C
6.66 - 9.52 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 18.0 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 87.0 - 97.0 kJ/m²41.4 - 46.2 ft-lb/in²Average value: 90.7 kJ/m² Grade Count:3
 89.0 - 92.0 kJ/m²
@Temperature -30.0 - -30.0 °C
42.4 - 43.8 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 90.3 kJ/m² Grade Count:3
Charpy Impact, Notched 0.700 - 0.700 J/cm²
@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.00 - 1.00e+14 ohm-cm5.00 - 1.00e+14 ohm-cmAverage value: 9.09e+12 ohm-cm Grade Count:11
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 - 220 °C424 - 428 °FAverage value: 219 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 210 - 232 °C410 - 450 °FAverage value: 220 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 98.9 - 227 °C210 - 440 °FAverage value: 204 °C Grade Count:11
Flammability, UL94 HBHBGrade Count:9
 
Processing PropertiesMetricEnglishComments
Processing Temperature 274 - 293 °C525 - 560 °FAverage value: 284 °C Grade Count:7
Melt Temperature 235 - 299 °C455 - 570 °FAverage value: 271 °C Grade Count:8
Mold Temperature 65.6 - 107 °C150 - 225 °FAverage value: 87.5 °C Grade Count:14
Drying Temperature 79.4 - 100 °C175 - 212 °FAverage value: 84.8 °C Grade Count:7
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 96.5 MPa Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 610, Glass Reinforced
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Overview of materials for Nylon 612, Impact Modified
Overview of materials for Nylon 11, Unreinforced

O2592 / 78044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.