MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger DELRIN® 500AF natural full strength POM-H, PTFE Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes:
  • low coefficient of friction
  • low static friction
  • excellent wear properties
  • excellent wear resistance
  • good machinability
  • high mechanical load capacity
Target Industries:
  • automotive industry
  • business machines
  • conveyor technology
  • gear manufacturing
  • heavy duty industry
  • printing machines
  • high mechanical load capacity
Target Industries:
  • packaging and paper machinery

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³
Moisture Absorption 0.110 %
@Time 86400 sec
0.110 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D 785
Hardness, Rockwell R 119119ASTM D 785
Hardness, Shore D 81.681.6ASTM D 2240
Tensile Strength, Yield 44.8 MPa6500 psiASTM D 638
Elongation at Break 6.5 %6.5 %ASTM D 638
Modulus of Elasticity 2.48 GPa360 ksiASTM D 638
Flexural Strength 76.67 MPa11120 psiASTM D 790
Flexural Modulus 3.34 GPa485 ksiASTM D 790
Compressive Yield Strength 96.5 MPa
@Strain 10 %
14000 psi
@Strain 10 %
ASTM D 695
Compressive Strength 22.6 MPa
@Strain 1 %
3280 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 1.844 GPa267.4 ksiASTM D 695
Izod Impact, Unnotched 0.320 J/cm0.600 ft-lb/inASTM D 256
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FDIN EN ISO 11357
Maximum Service Temperature, Air 85.0 °C185 °FLong Term
 149 °C300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FASTM D 648
 
Descriptive Properties
Colordark brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8136 / 319064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.