MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lutetium, Lu
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Silver Metal; Hexagonal

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.84 g/cc0.355 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 174.967174.9671995
Atomic Number 7171
X-ray Absorption Edge 0.19584 Å0.19584 ÅK
 1.14007 Å1.14007 ÅLI
 1.19745 Å1.19745 ÅLII
 1.34039 Å1.34039 ÅLIII
Electronegativity 1.01.0Pauling
Ionic Radius 0.850 Å0.850 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 4444
Tensile Strength, Ultimate 140 MPa20300 psi
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Break 12 %12 %
Tensile Modulus 68.6 GPa9950 ksi
Bulk Modulus 47.6 GPa6900 ksi
Poissons Ratio 0.2610.261
Shear Modulus 27.2 GPa3950 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000790 ohm-cm0.0000790 ohm-cm
Magnetic Susceptibility 1.02e-71.02e-7cgs/g
Critical Magnetic Field Strength, Oersted 350350
Critical Superconducting Temperature 0.0970 - 0.103 K0.0970 - 0.103 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 110 J/g47.3 BTU/lb
CTE, linear 9.90 µm/m-°C
@Temperature 20.0 °C
5.50 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.119 J/g-°C0.0284 BTU/lb-°FGas
 0.150 J/g-°C0.0359 BTU/lb-°F
Thermal Conductivity 16.4 W/m-K114 BTU-in/hr-ft²-°FPolycrystalline Sample
Melting Point 1651 - 1661 °C3004 - 3022 °F
Boiling Point 3402 °C6156 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 427.6 kJ/mol427.6 kJ/molGas
 
Component Elements PropertiesMetricEnglishComments
Lutetium, Lu 100 %100 %
 
Descriptive Properties
CAS Number7439-94-3
SolubilitySoluble in diluted Acid

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americium, Am
Silver, Ag
Chromium, Cr; Recrystallized
Aluminum, Al
Copper, Cu; Cold-Worked

AMELu00 / 55

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.