MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Styrolux® T SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrolux T is a new developmental, clear and tough styrene-butadiene copolymer (SBC) designed specifically for high performance film extrusion and shrink film applications. Styrolux T has been developped for blending with a second SBC component, Styrolux S, which inceases the stiffness of the film and improves the storage stability of film reels (reduced natural shrinkage).
  • Excellent clarity and toughness
  • Maximum shrinkage up to 80%
  • Very good shrinkage control
  • Very low gel content

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
ISO 62
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
11 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ISO 868
Tensile Strength, Yield 25.0 MPa3630 psiISO 527
Elongation at Break 250 %250 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 1.20 GPa174 ksiISO 527
Flexural Strength 32.0 MPa4640 psiISO 178
Flexural Modulus 1.00 GPa145 ksiISO 178
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  46.0 °C
@Load 5.10 kg
115 °F
@Load 11.2 lb
50°C/h; ISO 306
 62.0 °C
@Load 1.02 kg
144 °F
@Load 2.25 lb
50°C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D 1003
Transmission, Visible >= 89 %
@Wavelength 550 nm
>= 89 %
@Wavelength 550 nm
ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 230 °C356 - 446 °FISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Styrolux® HS 70 SBC
INEOS Styrolution Styrolux® S SBC
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
Ineos Nova 5470 High Impact Polystyrene
INEOS Styrolution Styrolux® 3G33 SBC

PBASF8028 / 159710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.