MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution PS 116 N/L GPPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.
  • Excellent flow properties
  • High heat resistance

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Melt Flow 23 g/10 min
@Load 5.00 kg,
Temperature 200 °C
23 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiISO 2039-1
Tensile Strength, Yield 40.0 MPa5800 psiISO 527
Elongation at Yield 1.5 %1.5 %ISO 527
Tensile Modulus 3.10 GPa450 ksiISO 527
Flexural Strength 70.0 MPa10200 psiISO 178
Charpy Impact Unnotched 0.900 J/cm²4.28 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75
Vicat Softening Point 85.0 °C
@Load 5.10 kg
185 °F
@Load 11.2 lb
120°C/h; ASTM D 1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 280 °C356 - 536 °FISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution PS 147F GPPS
INEOS Styrolution PS 124 N/L GPPS
INEOS Styrolution PS 1611 GPPS
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile

PBASG0568A / 159593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.