MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® X9408 High Impact PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material properties characterizing VESTODUR compounds are:
  • high thermostability
  • high stiffness
  • low water absorption resulting in high dimensional stability
  • high hardness
  • good strength
  • good sliding friction behavior, low abrasion
  • good creep behavior
  • good electrical properties
  • good chemical resistance
  • good weathering resistance
  • good processability
  • no tendency to form stress cracks

Specific Notes for this Material: Special types for different selective applications in the electrical, automotive, cable manufacturing, machine-building, and apparatus-construction industries. To some extent, the designations are synonyms for various product developments.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Linear Mold Shrinkage 0.020 cm/cm0.020 in/inPigmentation can change mold shrinkage.
Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inPigmentation can change mold shrinkage.
Melt Flow 18.15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
18.15 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; ISO 527-1/2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1/2
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527-1/2
Tensile Modulus 1.70 GPa247 ksiISO 527-1/2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inK20/P50; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 575 V575 VTest Solution A, 100 drops; IEC 60112
 >= 600 V>= 600 VTest Solution A, CTI; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C
@Temperature 23.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 150 µm/m-°C
@Temperature 23.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Melting Point 221 - 226 °C430 - 439 °FDSC
Vicat Softening Point 125 °C257 °F50N; ISO 306
 215 °C419 °F10N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural
Edinburg Plastics BTA706 PBT, Impact Modified

PHUMA77 / 47591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.