MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Cadmium Telluride (CdTe)
Categories: Ceramic; Sulfide/Chalcogenide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.86 g/cc0.212 lb/in³
Solubility 0.00 ppm0.00 ppm
a Lattice Constant 6.483 Å6.483 Å
Molecular Weight 240.01 g/mol240.01 g/mol
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 52.0 GPa7540 ksi
Poissons Ratio 0.410.41
Shear Modulus 18.4 GPa2670 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.50 µm/m-°C
@Temperature 0.000 - 30.0 °C
2.50 µin/in-°F
@Temperature 32.0 - 86.0 °F
Specific Heat Capacity 0.209 J/g-°C0.0500 BTU/lb-°F
Thermal Conductivity 4.10 W/m-K28.5 BTU-in/hr-ft²-°F
Melting Point 1092 °C1998 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.612.61n20.0
 2.6492.649n10.0
 2.598
@Wavelength 22000 nm
2.598
@Wavelength 22000 nm
 2.629
@Wavelength 16000 nm
2.629
@Wavelength 16000 nm
 2.649
@Wavelength 10000 nm
2.649
@Wavelength 10000 nm
 2.656
@Wavelength 6000 nm
2.656
@Wavelength 6000 nm
IR Transmittance  10 %
@Wavelength 800 nm
10 %
@Wavelength 800 nm
Internal Transmittance
 15 %
@Wavelength 35000 nm
15 %
@Wavelength 35000 nm
Internal Transmittance
 55 %
@Wavelength 950 nm
55 %
@Wavelength 950 nm
Internal Transmittance
 70 %
@Wavelength 15000 nm
70 %
@Wavelength 15000 nm
Internal Transmittance
 
Descriptive Properties
Absorption loss (cm^-1)0.167at 10 microns
Symmetrycubic
Symmetry ClassF43m
Transmission Range (microns)2 - 25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mateck CdTe
Cadmium Telluride, CdTe, Cubic
Cadmium Telluride, CdTe, Hexagonal
Aluminum 5083-H32; 5083-H323
Diamond, Synthetic

CMAT040 / 87724

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.