MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 GF 25 1 L black (4637) PA 6 Dry, 25% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: AKROMID B3 GF 25 1 L black (4637) is a 25% glass fiber reinforced and heat stabilized polyamide-blend with a reduced density compared to standard PA6 GF 25. Applications are mainly technical components in the automotive and electronic industry, where a weight and cost reduction is required.

Additive: Heat Stabilizer

Features:

  • Heat Stabilized
  • Low Density
Uses:
  • Automotive Application
  • Electrical/Electronic Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Filler Content 25 %25 %ISO 1172
Moisture Absorption 1.5 %
@Temperature 70.0 °C
1.5 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 275 °C
10 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1183
Spiral Flow 86.0 cm33.9 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psi5 [mm/min]; ISO 527-2
Elongation at Break 3.3 %3.3 %5 [mm/min]; ISO 527-2
Tensile Modulus 7.50 GPa1090 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched  6.70 J/cm²
@Temperature -30.0 °C
31.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.80 J/cm²
@Temperature 23.0 °C
32.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 217 °C423 °FUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 198 °C388 °FUnannealed; ISO 75/A
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Glow Wire Ignition Temperature 775 °C
@Thickness 0.800 mm
1430 °F
@Thickness 0.0315 in
IEC 60695-2-13
Glow Wire Flammability Index 750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Nozzle Temperature 270 - 290 °C518 - 554 °F
Zone 1 230 - 295 °C446 - 563 °F
Zone 2 230 - 295 °C446 - 563 °F
Zone 3 230 - 295 °C446 - 563 °F
Zone 4 230 - 295 °C446 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time <= 2.00 hour<= 2.00 hour
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 5.00 MPa725 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 15 S1 black (1270) PA 6 Dry, 15% Glass Filled
Bamberger Polymers Bapolene® 1072 Polyethylene, Injection Grade
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Nylon 6, Unreinforced

PAKRO285 / 182872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.