MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® A3 1 black (2417) PA 66 Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: Akromid A3 1 black (2417) is a heat stabilized, nonreinforced polyamide 6.6. Applications are housings and fixtures in automotive and electric industry.

Features:

  • Heat Stabilized
Uses:
  • Automotive Applications
  • Electrical/Electronic Applications
  • Housings

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption 2.9 - 3.1 %
@Temperature 70.0 °C
2.9 - 3.1 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 8.0 - 9.0 %8.0 - 9.0 %ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.023 cm/cm0.023 in/inISO 294-4
Spiral Flow 104 cm40.9 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 20 %>= 20 %50 [mm/min]; ISO 527-2
Elongation at Yield 4.5 %4.5 %ISO 527-2/50
Tensile Modulus 3.20 GPa464 ksiISO 527-2/1
Flexural Strength 110 MPa16000 psi2 mm/min; ISO 178
Flexural Modulus 2.80 GPa406 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 71.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
39.4 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Melting Point 262 °C504 °FDSC, 10K/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75-2/A
Flammability, UL94 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
Glow Wire Ignition Temperature 675 °C
@Thickness 1.60 mm
1250 °F
@Thickness 0.0630 in
IEC 60695-2-13
Glow Wire Flammability Index 750 °C
@Thickness 1.60 mm
1380 °F
@Thickness 0.0630 in
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black
EPICHEM PA 66 Polyamide 66
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned
Akro-Plastic Akromid® A3 1 natural PA 6.6 Dry
Akro-Plastic Akromid® A3 1 black (2417) PA 66 Conditioned

PAKRO109 / 182696

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.