MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-BOND® 360-208 Conductive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting EMI/RFI shielding compound and is effective even for designs requiring the use of a fillet as opposed to a flanged bead.

Applications: Typically include sealing EMI/RFI leaks around vents, windows, and machined surfaces; the bonding and shielding of conduit bulkhead passthroughs.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.60 - 4.40 g/cc3.60 - 4.40 g/cc
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Thickness >= 254 microns>= 10.0 mil
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 9.65 MPa
@Temperature 100 °C,
Time 2700 sec
1400 psi
@Temperature 212 °F,
Time 0.750 hour
Lap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.010 ohm-cm
@Temperature 100 °C,
Time 2700 sec
<= 0.010 ohm-cm
@Temperature 212 °F,
Time 0.750 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -62.0 °C-79.6 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 115 °C
0.250 hour
@Temperature 239 °F
 45.0 min
@Temperature 100 °C
0.750 hour
@Temperature 212 °F
 60.0 min
@Temperature 95.0 °C
1.00 hour
@Temperature 203 °F
 120 min
@Temperature 66.0 °C
2.00 hour
@Temperature 151 °F
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Pot Life 60 min60 min
Working Life 60.0 min60.0 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
BinderEpoxy
ConsistencyThick Paste
Coverage9.9 cm2 / g
FillerAg/Cu, Ag
Mix Ratio100:33

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME056 / 28278

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.