MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Global GPEI-210 10% Glass Filled Reinforced, Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 10% Glass Fiber

Material Notes: Information provided by Global Polymers Corporation.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 6.3 g/10 min
@Load 6.60 kg,
Temperature 337 °C
6.3 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 114 MPa16500 psiASTM D638
Flexural Modulus 4.48 GPa650 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
GEHR Plastics PEI Polyetherimide
Avient Edgetek® PI-1000 Polyetherimide (PEI)
AGC Fluon® C88AXMP-HT ETFE

PGLOBX16 / 42170

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.