MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Orion Engineered Carbons ECORAX® 1670 Carbon Black
Categories: Carbon; Carbon Black

Material Notes: Specialty black for tire treads and bodies that provide reduced rolling resistance

Information provided by Orion Engineered Carbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.310 g/cc0.0112 lb/in³Pour Density; ASTM D 1513
Oil Absorption 107 %107 %(ml/100 g); Compressed Sample; ASTM D 3493
 140 %140 %(ml/100 g); ASTM D 2414
Loss On Ignition <= 1.0 %<= 1.0 %Heating Loss; ASTM D 1509
Specific Surface Area 92 m²/g92 m²/gStatistical thickness surface area; ASTM D 6556
Iodine Absorption Number 100100mg/g; ASTM D 1510
 
Descriptive Properties
Fines< 7.0 %ASTM D 1508
Individual Pellet Hardness< 40 gASTM D 5230, average 1.4 - 1.7 mm
Sieve Residue< 500 ppmASTM D 1514
Tint104ASTM D 3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DowAksa AKSACA™ A-38 3K Continuous Carbon Fiber
Graphite, Carbon, C
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled

EORION919 / 159743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.