MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Trinseo Plexiglas® HFI10 Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, High Flow, Molded

Material Notes: Plexiglas® HFI10 is an impact modified thermoplastic acrylic resin formulated for injection molding. It has high melt flow, enhanced mold release properties and provides 10 times the impact resistance of standard acrylics while maintaining excellent optical properties. It offers an excellent balance between melt flow and increased resistance to breakage, while providing weatherability superior to that provided by other high-impact plastics. Supplemental moldflow simulation data is available.

Appearance: Clear/Transparent; Colors Available; Opaque; Translucent

Characteristics: High Flow; Scratch Resistant; High Clarity; Good Color Stability; Good Dimensional Stability; Low Shrinkage; Good Thermal Stability; Good UV Resistance; Good Weather Resistance; Good Toughness; High Impact Resistance

Applications: Appliances; Lighting Diffusers

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Water Absorption 0.40 %0.40 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0080 cm/cm0.0030 - 0.0080 in/inASTM D955
Melt Flow 3.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.3 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 3838ASTM D785
Tensile Strength, Ultimate 37.9 MPa5500 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Tensile Modulus 1.86 GPa270 ksiASTM D638
Flexural Strength <= 71.0 MPa<= 10300 psiASTM D790
Flexural Modulus 1.86 GPa270 ksiASTM D790
Izod Impact, Notched 0.481 J/cm0.900 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.216 W/m-K1.50 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C192 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °Fannealed; ASTM D648
Vicat Softening Point 82.8 °C181 °F50°C/hr; 50N; ASTM D1525
 93.9 °C201 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49
@Temperature 22.8 °C
1.49
@Temperature 73.0 °F
ND; ASTM D542
Haze <= 1.0 %
@Thickness 3.17 mm
<= 1.0 %
@Thickness 0.125 in
ASTM D1003
Transmission, Visible 90 %
@Thickness 3.17 mm
90 %
@Thickness 0.125 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V825 Acrylic
Arkema Oroglas® HFI-10 Acrylic, Impact Grade
Trinseo Plexiglas® DR® Acrylic
Trinseo Plexiglas® VM Acrylic
Covestro Makrolon® 2256 Polycarbonate

PARKG038 / 24392

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.