MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zoltek™ PX35 Type-48 Chopped Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK Type-48 chopped fibers provide excellent mechanical and electrical properties for reinforcement in thermoplastic molding compounds requiring high strength and modulus, low density, electrical conductivity, dimensional stability, low thermal expansion and excellent friction/wear properties. APPLICATIONS: Injection molding of articles for use as components in applications requiring static dissipation and/or EMI shielding. Such articles include electronic devices, dust handling equipment, and notebook computer enclosures. RECOMMENDED USE: PBT/PET, PA (nylon)

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.200 g/cc>= 0.00723 lb/in³unpacked
Moisture Absorption <= 0.300 %<= 0.300 %
 
Descriptive Properties
Compression Ratio (minimum)0.5
Fiber Length8 mm (nominal)
Fiber Sizing ChemistryPolyester
Sizing Content7.5% by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
Zoltek™ PX35 UD200 Uni-Directional Carbon Fabric
Sinotek Materials Packing Carbon Fiber with Graphite
Zoltek™ PX35 Continuous Tow Carbon Fiber
Zoltek™ PX30 MF/ME Milled Carbon Fiber

ECZO809 / 232276

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.