MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® CD145 PTFE Coagulated Dispersion Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); PTFE Powder

Material Notes: Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.17 g/cc2.17 g/cc
Bulk Density 0.500 g/cc0.0181 lb/in³
Particle Size 550 µm550 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 37.0 MPa5370 psiASTM D1457
Elongation at Break 310 %310 %ASTM D1457
 
Descriptive Properties
Max Reduction Ratio500
Relative Extrusion Pressure1.9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PFA Grade 345 Extrusion and Molding Resin
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Rogers Arlon CLTE-AT Commercial Ceramic PTFE
Rogers Arlon AD255 Woven Glass and PTFE
Chemours Teflon® TE 5373A-N PTFE granular molding resin

PAGC39 / 22998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.