MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Epoxy, Molded, Mineral Filled
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 - 2.14 g/cc0.0542 - 0.0773 lb/in³Average value: 1.92 g/cc Grade Count:21
Water Absorption 0.0260 - 0.0400 %0.0260 - 0.0400 %Average value: 0.0307 % Grade Count:3
 0.250 - 0.250 %
@Temperature 50.0 - 50.0 °C
0.250 - 0.250 %
@Temperature 122 - 122 °F
Average value: 0.250 % Grade Count:3
 0.250 - 0.250 %
@Time 173000 - 173000 sec
0.250 - 0.250 %
@Time 48.0 - 48.0 hour
Average value: 0.250 % Grade Count:3
Linear Mold Shrinkage 0.00200 - 0.00600 cm/cm0.00200 - 0.00600 in/inAverage value: 0.00438 cm/cm Grade Count:12
Spiral Flow 38.0 - 125 cm15.0 - 49.2 inAverage value: 82.0 cm Grade Count:16
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 65.0 - 75.065.0 - 75.0Average value: 68.3 Grade Count:3
Hardness, Shore D 74.0 - 97.074.0 - 97.0Average value: 80.8 Grade Count:13
Tensile Strength, Ultimate 30.0 - 97.0 MPa4350 - 14100 psiAverage value: 80.3 MPa Grade Count:20
Flexural Yield Strength 60.0 - 147 MPa8700 - 21300 psiAverage value: 117 MPa Grade Count:21
Flexural Modulus 13.4 - 19.3 GPa1950 - 2800 ksiAverage value: 16.0 GPa Grade Count:11
Compressive Yield Strength 60.0 - 283 MPa8700 - 41000 psiAverage value: 216 MPa Grade Count:14
Izod Impact, Notched 0.160 - 0.320 J/cm0.300 - 0.600 ft-lb/inAverage value: 0.246 J/cm Grade Count:9
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 5.00e+16 ohm-cm1.00e+13 - 5.00e+16 ohm-cmAverage value: 1.25e+16 ohm-cm Grade Count:11
Surface Resistance 1.00e+12 - 1.00e+16 ohm1.00e+12 - 1.00e+16 ohmAverage value: 5.46e+15 ohm Grade Count:12
Dielectric Constant 3.50 - 5.603.50 - 5.60Average value: 4.39 Grade Count:21
Dielectric Strength 13.8 - 20.0 kV/mm350 - 508 kV/inAverage value: 15.8 kV/mm Grade Count:20
Dielectric Breakdown 56.0 - 60.0 V56.0 - 60.0 VAverage value: 58.7 V Grade Count:3
 >= 30000 V
@Temperature 90.0 - 90.0 °C
>= 30000 V
@Temperature 194 - 194 °F
Average value: 30000 V Grade Count:1
 >= 30000 V
@Time 20.0 - 60.0 sec
>= 30000 V
@Time 0.00556 - 0.0167 hour
Average value: 30000 V Grade Count:1
Dissipation Factor 0.00100 - 0.04000.00100 - 0.0400Average value: 0.00938 Grade Count:21
Dielectric Loss Index 0.0110 - 0.03200.0110 - 0.0320Average value: 0.0200 Grade Count:6
Arc Resistance 18.0 - 210 sec18.0 - 210 secAverage value: 177 sec Grade Count:18
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.0 - 92.0 µm/m-°C11.7 - 51.1 µin/in-°FAverage value: 44.4 µm/m-°C Grade Count:16
CTE, linear, Transverse to Flow 69.0 - 90.0 µm/m-°C38.3 - 50.0 µin/in-°FAverage value: 75.1 µm/m-°C Grade Count:7
Thermal Conductivity 0.0418 - 16.0 W/m-K0.290 - 111 BTU-in/hr-ft²-°FAverage value: 1.63 W/m-K Grade Count:17
Maximum Service Temperature, Air 190 - 200 °C374 - 392 °FAverage value: 196 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 100 - 110 °C212 - 230 °FAverage value: 106 °C Grade Count:4
Heat Distortion Temperature 260 °C500 °FAverage value: 260 °C Grade Count:3
Glass Transition Temp, Tg 130 - 175 °C266 - 347 °FAverage value: 156 °C Grade Count:17
Flammability, UL94 HB - V-0HB - V-0Grade Count:16
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 193 °C338 - 379 °FAverage value: 180 °C Grade Count:7
Mold Temperature 145 - 180 °C293 - 356 °FAverage value: 164 °C Grade Count:12
Cure Time 0.450 - 240 min
@Temperature 150 - 150 °C
0.00750 - 4.00 hour
@Temperature 302 - 302 °F
Average value: 14.5 min Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
Overview of materials for Solventless Epoxy Varnish, Electrical Insulation
Overview of materials for Epoxy, High Temperature

O1706 / 77891

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.