MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD 3485-3 Liquid Crystal Polymer (LCP), Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Carbon Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D 792
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.00 - 0.00020 cm/cm
@Thickness 3.20 mm
0.00 - 0.00020 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 152 MPa22000 psiASTM D 638
Elongation at Break 1.0 %1.0 %ASTM D 638
Tensile Modulus 34.5 GPa5000 ksiASTM D 638
Flexural Strength 231 MPa33500 psiASTM D 790
Flexural Modulus 24.1 GPa3500 ksiASTM D 790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.20 mm
1.30 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 3.74 J/cm
@Thickness 3.20 mm
7.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmASTM D 257
Surface Resistance <= 10000 ohm<= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  40 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
40 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 40 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
40 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 40 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
40 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 41 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
41 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 42 dB
@Thickness 2.00 mm,
Frequency 1.50e+8 Hz
42 dB
@Thickness 0.0787 in,
Frequency 1.50e+8 Hz
ASTM D 4935
 43 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
43 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 43 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
43 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 45 dB
@Thickness 2.00 mm,
Frequency 3.00e+7 Hz
45 dB
@Thickness 0.0787 in,
Frequency 3.00e+7 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 285 °C545 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 332 - 366 °C630 - 690 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 149 °C
@Time 28800 sec
300 °F
@Time 8.00 hour
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZPA45727 / 279731

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.