MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Canuck Compounders BK 8-8-7RUV Black, UV Stabilized TPO
Categories: Polymer; Thermoplastic; TPO, Unfilled (not elastomer)

Material Notes: Material Status: Commercial: Active, Availability: North America, Forms: Pellets.

Information provided by Canuck Compounders, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D 792
Filler Content 7.0 %7.0 %ASTM D4218
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 230 °C
32 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiISO 527
Flexural Modulus 1.15 GPa167 ksiISO 178
Izod Impact, Notched (ISO)  4.50 kJ/m²
@Temperature -40.0 °C
2.14 ft-lb/in²
@Temperature -40.0 °F
ISO 179A
 44.0 kJ/m²
@Temperature 23.0 °C
20.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Buckeye Polymers BP FLEX D 6509 CR Injection Grade TPO
Buckeye Polymers BP FLEX D 6020 Injection Grade TPO
Buckeye Polymers BP FLEX D 5608 T Injection Grade TPO
Buckeye Polymers BP FLEX D 5518 Injection Grade TPO
Buckeye Polymers BP FLEX D 4107 Injection Grade TPO

PCANUCK915 / 218620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.